You do not have permission to edit this page, for the following reason:
Training guide {{SeedNotice}} = Ceramics Room Orientation and Procedures = <div class="cs-notice">'''Required before equipment use:''' Complete a steward-led onboarding session. The source deck warns: '''no food in the Ceramics room; clay dust and glazes are toxic.''' Never pour clay, slip, or glaze down the sink.</div> This page consolidates the CreatorSpace ceramics procedure deck into a searchable orientation guide. Slides 2-3 and 4-5 are duplicate revisions, so each topic appears once here. Check posted labels and current steward directions before beginning work. {{#ifexist:File:Ceramics-room-procedures.pdf|[[:File:Ceramics-room-procedures.pdf|View or download the original 12-slide Ceramic Procedures deck (PDF)]].|The original 12-slide deck is preserved in the project seed assets; this page contains its consolidated procedures.}} == Contacts and Onboarding == * '''Steward:''' Mel Gromek * '''Co-steward:''' Rachel Gamblin * Direct-message the ceramics steward on Slack to schedule an onboarding session. * Complete onboarding before using any ceramics equipment. * Direct-message Mel with questions about a procedure or project. == Clay Vocabulary == Label work in progress with the correct term. {| class="wikitable" ! Term ! Meaning |- | '''Wet / plastic clay''' | Freshly shaped clay that can be altered, repaired easily, or reused. |- | '''Leather-hard clay''' | Partly dry clay, ideal for carving, trimming, and adding. It can still be reused or recycled. |- | '''Greenware''' | Non-fired, bone-dry clay with no moisture. It is very fragile and can still be recycled. |- | '''Bisqueware''' | Clay that has been fired once but not glazed. It is glazed after the bisque firing and then fired again. |} == General Equipment Procedures == * Sign in with your name and date before using equipment. * Room capacity is '''six people'''. * Reserve a wheel with your name, date, and time. * Use only the clay supplied in the room's buckets. The source deck identifies the standard clay as white stoneware. * Ask a steward before using an alternate clay. * Weigh your clay and record the amount on the sign-in sheet. * Begin by wedging the clay to remove air bubbles. == Wheel Throwing == === Prepare the Clay === * Wedge the clay first. * For a small bowl, plate, or mug, form a round clay ball of approximately '''1-2 lb'''. === Wheel Direction === * Use the wheel's direction switch for left- or right-handed throwing. * Right-handed throwing spins counterclockwise. * Left-handed throwing spins clockwise. === Slip and Cleanup === '''Slip''' is the muddy water on the wheel that falls into the tray. It can act like glue when attaching handles and decorative pieces. * Use your own slip bucket, label it with your name, and cover it when finished. * Remove your discarded clay. * Carefully skim off water so the slip clay can be reused for hand building or attaching pieces. * Do not reuse slip or used clay for another pottery-wheel session. * Never pour clay or slip down the sink; it will clog the drain. * Wash and wipe the wheel, floor, and window. * Allow '''15 minutes''' for cleanup. * Turn off the wheel when finished. == Storing Thrown Pieces == === On the Day You Throw === # Move each piece from the work area onto a board. # Cover the piece loosely with plastic wrap. # Put a name tag on or inside the plastic wrap. # Put the board and piece in the metal cabinet. Trim the bottom later. === At Leather Hard - Approximately 24 Hours === # Trim the bottom. # Sign the piece with a stamp or scraping tool. # Put the completed piece, uncovered, in the metal cabinet to dry fully. Full drying takes about one week. The source deck says the studio needs at least '''20-30 pieces''' for a bisque firing. Tools are stored in labeled drawers. Put the tools you need in a plastic container, wash them carefully after use, and let them dry on the rack before putting them away. == Hand Building == * Wedge all clay before hand building, using the wedging table on the right side of the room. * Draw the planned piece and keep notes. * Use canvas to roll out a slab; firm clay is easier to build with. * Metal cookie cutters or metal/plastic containers can be used as forms. * Make coils and other construction parts first, then let the clay firm for about '''30 minutes'''. * Do not leave work on the shared table. * Clean tools and return canvas and aprons to their hooks. <div class="cs-notice">'''Needs steward confirmation:''' The source slide says, "Spray lightly with vegetable to avoid sticking," but it does not name the intended product. Confirm the current mold-release practice before applying anything to a form.</div> If you finish or run out of time: # Put the pieces on a board and add your name and date on tape. # Cover them well and place them in the metal cabinet. # Return within two weeks; unfinished pieces left longer than two weeks will be discarded. == Glazing == === Before You Apply Glaze === * Read the label on every glaze container first. * Most glazes go only on bisqueware; follow the jar instructions. * Usually three coats are required. Let each coat dry. * Some underglazes can be used on greenware. * Do not put an underglaze over a glaze. * Mix glaze thoroughly with a metal spoon before use. * If the glaze is very thick or hard, add only a small amount of water. The source compares the intended consistency to Elmer's glue or a yogurt shake. === Dispensing and Application === * Pour only enough glaze for your piece into a small cup. * Do not mix two glazes together in that container. * Use a different brush and a clean spoon for each glaze jar. * A little water can create a watercolor-like wash. * Ask the steward about layering glazes. * When finished, return the remaining glaze to its original jar using the spoon and brush, as directed in the source deck. === Protect the Kiln === * Remove all glaze from the bottom of the piece with a wet sponge. * Also clean approximately '''1/4 inch''' up the bottom sides because some glazes run. * Clay "cookies" are available to place under pots. * Clean each piece thoroughly to avoid damaging the kiln. === Notes, Spills, and the Firing Queue === * Record each glaze and the number of coats used. * Consult the glaze manufacturer's instructions for application guidance and intended results. * Use the studio's display tiles for examples. Most available glazes are described as mid-fire, cone 5-6. * Clean glaze spills immediately with a scrubbing motion. * Thoroughly rinse brushes, utensils, and containers with water, then let brushes dry brush-side up in the buckets. * Never pour glaze down the sink. * Put the glazed piece on a board, then on the bookshelf to await glaze firing. * The deck estimates that the firing wait can be about three weeks, but marks that timing as uncertain. Ask the steward for the current queue estimate. == Glaze Firing and Cone Reference == <div class="cs-notice">'''Reference only:''' This orientation does not authorize kiln operation. Complete [[Training/Kiln Orientation|Kiln Orientation]] and follow the kiln steward's current loading and firing procedures.</div> * Read the Orton cone chart as a pyrometric temperature/heatwork reference. * Pyrometric cones sit on kiln shelves and bend as the required heatwork is reached; both temperature and time matter. * Every clay body and glaze is designed for a particular cone value or range. * Record the required firing cone for each piece. {| class="wikitable" ! Glaze category ! Matching clay and cone range ! Temperature range in the source deck |- | Low-fire | Low-fire clay, cone 06-04 | 1,830-1,940 °F |- | Mid-range | Mid-range clay, cone 4-6 | 2,167-2,232 °F |- | High-fire | High-fire clay, cone 8-10 | 2,305-2,345 °F |} The deck describes most current glazes as cone 5-6 and mentions high-fire capability as a future hope, not a current authorization. == Using Plaster Molds == The plaster molds are stored in the '''Hot Shed''' in the rear parking lot. Ask a steward which mold-specific instructions or video apply before starting. === Fill the Mold === # Stir the pouring slip well. # Use a measuring cup to pour slip into the mold. # Replace the pouring-slip lid after taking the amount you need. # Let the slip set well before removing it. As it dries, it pulls away from the mold walls. Some molds are difficult to release; follow the steward-approved instructions for that mold. === Store and Dry the Piece === # Put the unmolded piece on a board and cover it well with plastic. # Sign the piece and attach a label with your name and date. # Put it in the metal cabinet. If it is too tall, use the Hot Shed storage area. # Let clay dry slowly; never put the piece in direct sun. # Return the plaster mold to the Hot Shed. == Source and Review Notes == * Source: 12-slide Ceramic Procedures deck; PDF metadata creation date October 8, 2026. {{#ifexist:File:Ceramics-room-procedures.pdf|[[:File:Ceramics-room-procedures.pdf|Open the source PDF.]]|The original PDF is preserved in the project seed media.}} * Duplicate vocabulary and equipment slides were consolidated into one copy of each procedure. * Obvious grammar and spelling errors were normalized without changing the stated process. * The incomplete "spray lightly with vegetable" instruction remains flagged for steward clarification. * Before approval, stewards should confirm contacts, room capacity, clay stock, sink and reclaim practice, glaze-return practice, firing queue, cone capability, and plaster-mold instructions. [[Category:CreatorSpace POC]]